ASTM A139 Grade B EFW -buizen
ASTM A139 Grade B EFW -buizen Beschrijving
ASTM A139 LaDed Pipe is een elektrische fusie (ARC) gelaste spiraalvormige stalen pijp gespecificeerd door de American Society for Testing and Materials (ASTM). Het is een stalen pijp met een nominale diameter van NPS 8 tot 142 (ongeveer 219 mm tot 3620 mm) en een wanddikte van 1,0 inch (25,4 mm). De nieuwste versie van de ASTM A139-standaard is ASTM A139/A139M-22, die de vorige versies van 2004 en 2015 vervangt.
Toepassingscapaciteit
Gebruikt om vloeistoffen, gassen of stoom te transporteren, zoals kraanwater, olie, aardgas, stoom, enz.
Bedekt rechte naad- of spiraalvormige lasstalen buizen, de stalen kwaliteit is een speciaal graad voor stalen pijpfabrieken en de mechanische eigenschappen verschillen van standaard stalen platen.
Hoofdparameters
Buisdiameter: NPS 8 tot 142 (zie ANSI B36.10 voor specifieke afmetingen).
Wanddikte: nominale (gemiddelde) wanddikte minder dan of gelijk aan 1,0 inch (25,4 mm).
Staalkwaliteit: verdeeld in vijf graden, die moeten voldoen aan specifieke mechanische eigenschappen zoals treksterkte en opbrengststerkte.
Productieproces
Het lasproces voor elektrische smeltmels (ARC) wordt aangenomen en de lassen moeten strikte inspecties doorstaan, zoals röntgenfoutdetectie en ultrasone tests.
Het productieproces omvat stappen zoals stripfrezen, vormen, lassen en waterdruk testen om de kwaliteit van de lassen te waarborgen.
Toepassingsgebieden
- Gemeentelijke engineering: kraanwater, drainage en verwarmingspijpleidingen.
- Industriële velden: petrochemische, kracht- en chemische pijpleidingen.
- Structureel gebruik: bruggen, dokken, bouwsteunen, etc.
ASTM A139 Grade B EFW -buizen Specificatie
ASTM A139 GRB gelaste pijpen chemische samenstelling
| C | Mn | P | S | |
|---|---|---|---|---|
| Grade B: | .26 | 1.00 | .035 | .035 |
ASTM A139 GRB EFW -stalen buizen leveren en treksterkte op
| Minimale opbrengst | Minimale trek | |
|---|---|---|
| Grade B: | 35.000 psi | 60.000 psi |
EFW A139 GRB Koolstofstaalpijpgroottekaart
| Pijpen/ buistype | NB -maten | SCH 5 | Sch 10 | SCH 40 | SCH 80 | SCH 160 |
|---|---|---|---|---|---|---|
| ASTM A139 gelast | 1/2 | ✔ | ✔ | ✔ | ✔ | |
| ASTM A139 gelast | 3/4 | ✔ | ✔ | ✔ | ✔ | |
| ASTM A139 gelast | 1 | ✔ | ✔ | ✔ | ✔ | |
| ASTM A139 gelast | 1.25 | ✔ | ✔ | ✔ | ✔ | ✔ |
| ASTM A139 gelast | 1.5 | ✔ | ✔ | ✔ | ✔ | ✔ |
| ASTM A139 gelast | 2 | ✔ | ✔ | ✔ | ✔ | ✔ |
| ASTM A139 gelast | 2.5 | ✔ | ✔ | ✔ | ✔ | ✔ |
| ASTM A139 gelast | 3 | ✔ | ✔ | ✔ | ✔ | ✔ |
| ASTM A139 gelast | 3.5 | ✔ | ✔ | ✔ | ✔ | ✔ |
| ASTM A139 gelast | 4 | ✔ | ✔ | ✔ | ✔ | ✔ |
| ASTM A139 gelast | 5 | ✔ | ✔ | ✔ | ✔ | ✔ |
| ASTM A139 gelast | 6 | ✔ | ✔ | ✔ | ✔ | ✔ |
| ASTM A139 gelast | 8 | ✔ | ✔ | ✔ | ✔ | ✔ |
| ASTM A139 gelast | 10 | ✔ | ✔ | ✔ | ✔ | ✔ |
| ASTM A139 gelast | 12 | ✔ | ✔ | ✔ | ✔ | ✔ |
| ASTM A139 gelast | 14 | ✔ | ✔ | ✔ | ✔ | ✔ |
| ASTM A139 gelast | 16 | ✔ | ✔ | ✔ | ✔ | ✔ |
| ASTM A139 gelast | 18 | ✔ | ✔ | ✔ | ✔ | ✔ |
| ASTM A139 gelast | 20 | ✔ | ✔ | ✔ | ✔ | ✔ |
| ASTM A139 gelast | 22 | ✔ | ✔ | ✔ | ✔ | |
| ASTM A139 gelast | 24 | ✔ | ✔ | ✔ | ✔ |
ASTM A139 Grade B EFW -buizen op voorraad
Gnee Group produceert jaarlijks 500 ton A139 gelaste pijpen.



Over Gnee
Gnee Group werd opgericht in 2008 en houdt zich bezig met de productie en export van gelaste pijpen. Om de kwaliteit van stalen buizen te waarborgen, is GNEE-fabriek uitgerust met professionele en volledige testapparatuur, waaronder: directe leesspectrometer, drop hammer impact testmachine, snel intelligente zwavelbepaling, elektronische universele testmachine, röntgendetectie, ultrasone detectie, enz. Met hoogwaardige gelaste pijpen en zorgvuldige service is Gnee Group de voorkeursleverancier van grote engineeringprojecten in binnen- en buitenland geworden. Gnee Group ontvangt ook elk jaar tentoonstellingssamenwerking uitnodigingen uit Vietnam, Indonesië, Rusland en andere landen.
Inspectieapparatuur van stalen buis

Tentoonstelling Samenwerking

Populaire tags: ASTM A139 Grade B EFW -buizen, China ASTM A139 Grade B EFW -buizen Fabrikanten, leveranciers
Volgende
ASTM A134 EFW stalen buizenMisschien vind je dit ook leuk
Aanvraag sturen