| Specificatie | Dikte | kg/stuk (6 meter) | Specificatie | Dikte | kg/stuk (6 meter) |
| DN15 (4 cent) |
2.00 | 5.58 | DN80 (3 inch) |
3.00 | 38.05 |
| 2.20 | 6.10 | 3.25 | 40.75 | ||
| 2.50 | 6.90 | 3.50 | 44.95 | ||
| 2.75 | 7.45 | 3.75 | 47.15 | ||
| DN20 (6 cent) |
1.80 | 6.31 | 4.00 | 51.50 | |
| 2.00 | 6.95 | DN100 (4 inch) |
3.00 | 49.48 | |
| 2.20 | 7.90 | 3.25 | 53.15 | ||
| 2.50 | 8.94 | 3.50 | 57.55 | ||
| 2.75 | 9.73 | 3.75 | 61.65 | ||
| DN25 (1 inch) |
2.20 | 10.27 | 4.00 | 65.50 | |
| 2.50 | 11.42 | DN125 (5 inch) |
3.50 | 71.35 | |
| 2.75 | 12.45 | 3.75 | 75.68 | ||
| 3.00 | 13.75 | 4.00 | 81.40 | ||
| 3.25 | 14.50 | 4.25 | 85.85 | ||
| DN32 (1,2 inch) |
2.20 | 13.51 | 4.50 | 91.25 | |
| 2.50 | 14.80 | DN150 (6 inch) |
3.50 | 83.86 | |
| 2.75 | 16.00 | 3.75 | 91.89 | ||
| 3.00 | 17.68 | 4.00 | 97.58 | ||
| 3.25 | 18.80 | 4.25 | 103.46 | ||
| DN40 (1,5 inch) |
2.50 | 16.88 | 4.50 | 108.78 | |
| 2.75 | 18.35 | DN200 (8 inch) |
5.00 | 161.95 | |
| 3.00 | 20.00 | 5.25 | 166.00 | ||
| 3.25 | 21.95 | 5.50 | 178.05 | ||
| 3.50 | 23.55 | 5.75 | 187.38 | ||
| DN50 (2 inch) |
2.50 | 21.25 | 6.00 | 194.85 | |
| 2.75 | 23.35 | DN250 (10 inch) |
5.00 | 201.00 | |
| 3.00 | 25.62 | 5.25 | 209.00 | ||
| 3.25 | 28.18 | 5.50 | 223.00 | ||
| 3.50 | 30.15 | 5.75 | 232.15 | ||
| DN65 (2,5 inch) |
2.75 | 29.85 | 6.00 | 239.64 | |
| 3.00 | 33.95 | DN300 (12 inch) |
5.00 | 239.58 | |
| 3.25 | 35.45 | 5.25 | 249.30 | ||
| 3.50 | 37.50 | 5.50 | 263.33 | ||
| 3.75 | 41.15 | 5.75 | 275.70 | ||
| 6.00 | 286.30 | ||||
Als u maatwerk nodig heeft, kunt u altijd contact met ons opnemen. Wij produceren stalen buizen met andere specificaties volgens uw vereisten.